public catalogue · open access · last index pass 2026-06-30 08:14:02 UTChost: cat-pub-04 · build 0.14.3-prototype · rev rA9F2
overviewcatalogueAM-2012-10017-A

AM-2012-10017-A · Cupritearchived

physical & structuralrev. 2
designationCuprite
chemical formulaCu₂O
classificationOxide
crystal systemCubic
mohs hardness3.5 – 4
density (g/cm³)6.13
colourBrick red
type localityKashio mine, Nagano, Japan
raman spectroscopy532 nm · pass A
200400600800100012001400Raman shift (cm⁻¹)intensity (arb.)147413634
λ_excitation: 532 nm · acq. 3 × 10 s · grating 1800 g/mmfig. 1 · raman.am-2012-10017-a.svg

reported peaks (cm⁻¹): 147, 413, 634

notessubmitter remarks + registry

Photographic record retained. Specimen temperature held at lab ambient throughout intake.

chain of custody8 events · 5 seal-breaks

Events recorded against this accession in the registry's printed custody book. Operator initials are anonymous. Storage codes follow the convention vault-shelf-drawer.

timestampstagedetailop.
2012-07-17 08:27 UTCintakeweighed, dimensioned, photographed; container sealed and labelled with the accession identifierT.J.
2012-07-19 10:07 UTCpass Avisual inspection · density (Archimedes) · mass to ±0.01 gM.A.
2012-07-24 09:33 UTCpass BRaman acquisition; 3 peaks above prominence threshold
instrument: Horiba LabRAM HR (532 nm)
ref. checked: RRUFF R05008
M.A.
2012-07-25 11:41 UTCstoragere-bagged, label re-printed; placed in vault D, shelf 23, drawer 35T.J.
2014-07-25 09:03 UTCre-inspectionseal intact · label legible · no visible degradationN.P.
2016-07-24 13:41 UTCre-inspectionseal intact · label legible · no visible degradationN.P.
2018-07-24 16:38 UTCre-inspectionseal intact · label legible · no visible degradationN.P.
2020-07-23 09:34 UTCre-inspectionseal intact · label legible · no visible degradationN.P.

physical location: vault D · shelf 23 · drawer 35 · last documented inspection: 2020-07-23 09:34 UTC